水磨石地坪不够亮的原因及解决方法

2018-11-04 18:32:49 常州市星火铝艺制品有限公司 阅读

水磨石环氧地坪因为花色可随意拼接、施工方便、造价低廉等特性广受欢迎,从最开始的工业领域到如今的商业领域,水磨石环氧地坪的热度一直不见减少,在超市、商场、饭店以及家装都场所都能看到它的身影。光亮度一直是水磨石地面的一个很亮眼的特点,可以说,大部分还是很喜欢水磨石地坪的花色和光亮度,所以才是选择做水磨石地坪。不过有的时候水磨石地面在施工完成后会出现表面黯淡,光泽度明显达不到标准的的问题。至于为什么会出现这样的问题,绝大多数人都是不明所以。下面小编就简单讲讲水磨石地面光亮度差的原因以及解决方法。

Terrazzo floors are popular because of the characteristics of freely splicing, convenient construction and low cost. From the beginning of the industrial field to today's commercial field, the heat of terrazzo floors has not been reduced. It can be seen in supermarkets, shopping malls, restaurants and home furnishings. Brightness has always been a very bright feature of terrazzo floors. It can be said that most of them still like the color and brightness of terrazzo floors, so they choose to be terrazzo floors. However, sometimes the terrazzo surface will be dim after the completion of construction, and the gloss can not reach the standard obviously. As for why such a problem occurs, most people are not aware of it. The following is a brief introduction to the reasons for the poor brightness of terrazzo floor and the solution. 

一、水磨石地面光亮度差的原因

1. Reasons for poor brightness of terrazzo floor

1、磨光时磨石规格不齐,使用不当

1. When grinding, the specifications of the grindstone are uneven.

水磨石地面在施工时,磨光次数一般不应少于3次。不过在施工中,用到的禁房事砂轮往往规格不齐,并且对第二遍和第三遍的磨石要求不够重视,只要求石子、分隔条清晰可见,却忽略了对表面光亮度的施工要求。

In the construction of terrazzo floor, the frequency of polishing should not be less than 3 times. However, in construction, the specifications of forbidden grinding wheels used are often uneven, and the second and third times of grinding stone requirements are not enough attention, as long as the stone, separator bars are clearly visible, but the construction requirements of surface brightness are ignored.

2、打蜡钱没有涂抹草酸溶液

2, waxing money did not apply oxalic acid solution.

水磨石地面在打蜡前都是要涂抹草酸溶液的,并且如果不是涂抹溶液而是用粉状草酸进行干擦的话,会很难保证草酸在地面的均匀性。擦洗后,地面表面的洁净程度不一致,没擦干净的地方就会出现斑痕,直接影响打蜡的效果,造成水磨石地面光亮度低。

The terrazzo floor is coated with oxalic acid solution before waxing, and it is difficult to ensure the homogeneity of oxalic acid on the ground if it is not coated with oxalic acid solution but dried with powder oxalic acid. After scrubbing, the cleanliness of the ground surface is inconsistent, and there will be spots where it is not cleaned, which directly affects the effect of waxing, resulting in low brightness of terrazzo ground.

3、使用刷浆法来补浆

3. Use the brush method to reinforce the pulp.

刷浆法补浆的缺点在于无法完全消除洞眼,只会在洞眼上下形成一层薄膜,在打磨后洞眼依然存在,这会导致水磨石地面光亮度低。

The disadvantage of grouting by brushing method is that it can not eliminate the holes completely, but only form a layer of film above and below the holes. After polishing, the holes still exist, which will lead to low brightness of terrazzo floor.

二、水磨石地坪光亮度差的解决方法

Two. Solution to the difference of terrazzo floor brightness.

水磨石光亮度差并不需要敲掉重新施工,只需要使用混凝土密封固化剂就可以提升地面的光亮度。混凝土密封固化剂可以封堵住水磨石地面表面的孔隙,使之成为一个密实的整体,再使用专业的打磨机器多层次打磨后,可以让地面呈现出大理石般的光泽。并且会随着使用时间的增加,光泽度也会增加。

The difference in brightness of terrazzo does not need to be knocked out and re-constructed, but only the use of concrete sealant curing agent can improve the brightness of the ground. The concrete sealing solidifying agent can block the pore of terrazzo surface and make it a compact whole. After multi-level polishing with professional polishing machine, the terrazzo surface can show marble-like luster. And the gloss will also increase with the increase of use time.

除了能够增亮水磨石地面,混凝土密封固化剂还能达到硬化、强固、抗磨耗、防尘、防水、抗化学侵蚀、抗盐分、抗油污、安全环保的固封效果,还能增加地坪的使用寿命,最高可达30年。

In addition to brightening terrazzo floors, concrete sealants can also achieve hardening, strong, anti-wear, dust-proof, waterproof, chemical erosion resistance, salt resistance, oil pollution resistance, safety and environmental protection of the sealing effect, but also increase the service life of the floor, up to 30 years.